Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.00e+7 ohm-cm | >= 1.00e+7 ohm-cm | ASTM D257 |
Polikim EFALON® B-60 PTFE, 60% Bronze Filled Bronze-filled Efalon® (PTFE) has better heat insulation, less thermal expansion, higher wear resistance properties and less deformation under load compared to virgin Efalon®. Applications: bearing.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 93 |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific) Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 1V; IEC 60093 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PC CF20 CR X 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Good Chemical Resistance and Semi ConductiveInformation provided by TP Compos.. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+9 ohm-cm | 1.00e+7 - 1.00e+9 ohm-cm | ASTM D257 |
Techmer ES Statiblend® POM CO AS BK Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Lubrizol Hipscon™ M-505 Static Control High Impact Polystyrene Hipscon™ M-505 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are lightweight and easily formed into deep pockets that maintain unifo.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Lubrizol Hipscon™ M-520 Static Control High Impact Polystyrene Hipscon™ M-520 is a conductive, carbon black filled, High Impact Polystyrene available as extruded sheet. Thermoformed trays are easily formed into deep pockets that maintain uniform static protec.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW300 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW371 (COND) Nylon 46 Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 805 PTFE, 40% Bronze Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2 Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 812 PTFE, 46% Bronze, Green Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2 Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Adamas Adalon® 816 PTFE, 46% Bronze, Blue Information provided by Adamas, HPM |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
DSM Stanyl® TW200F3 (COND) Nylon 46 15% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | IEC 60093 |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Volume Resistivity | <= 1.00e+7 ohm-cm | <= 1.00e+7 ohm-cm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Volume Resistivity | 1.00e+7 ohm-cm | 1.00e+7 ohm-cm | 1V; IEC 60093 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |