Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Network Polymers Kepital® F20-25 Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Kolon Kocetal® CL704 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
DSM Akulon® K224-PG2U (Dry) 13% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **)&l Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
DSM Akulon® K223-HMS6 Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | 150°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-b Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | |
Mikro-Technik Mikrolen UHMW-PE Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26.. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | IEC 60093 |
Lanxess Pocan® B 1501 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | NBR 5403 |
Karina 10/96-FC-LMP White Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Volume Resistivity | >= 1.00e+14 ohm-cm | >= 1.00e+14 ohm-cm | NBR 5403 |
Karina E 48/1-FC-LMP Black Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. Important Con.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PA6/6 GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | DIN 53482 |
Polyram PlusTek RA843 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
Cotronics Duralco™ 4538N Super Flexible Epoxy, Room Temperature Cure Rubber-like epoxy that has the flexible of a silicone and the chemical stability of an epoxy. It adheres to most plastics, metals, ceramics, glass, rubber and even treated Teflon™. Cures at room .. |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 23.0 °C |
1.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds AP 87/1 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural Information provided by Eurotec® |
|||
Volume Resistivity | 1.00e+14 ohm-cm @Temperature 20.0 °C |
1.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 3621 Halogen Free PVC General purpose |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
3M Scotch® 31 Heavy Duty Mining Tape Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D247 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | IEC 60093 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |