Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Plastcom SLOVAMID 66 OB PA66, optically brightened FeaturesPA 66 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and modulus of elasticity in tension in comparison with the basic type... |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Polimeri Europa SINKRAL B813 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, providing very high impact resistance, even at low temperatures. Used as.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | VDE 0303 |
GEHR Plastics PA 6.6-30GF Nylon 6.6, 30% Glass Fiber, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
Menzolit Menzolit® BMC 1000 Unsaturated Polyester UP BMC 1000 is a special BMC for hydrolysis resistant applications. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. Typical applic.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243 |
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243 |
Teijin Panlite® LV-2250Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required for normal fluidity.Applications:.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | VDE 0303/4 |
Polyram RamSter PF702 PBT, UV Stabilized UV stabilized, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | JIS K2111 |
Toyobo Pelprene™ P-150M Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm |
762 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Makrolon® 2808 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Covestro Makrolon® 9125 Polycarbonate Medium viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | dry; IEC 60243-1 |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | dry; IEC 60243-1 |
DSM Stanyl® TC153 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Dielectric Strength | >= 30.0 kV/mm | >= 762 kV/in | No thickness given; ASTM D877 |
ConocoPhillips Hydroclear® 68 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | |
Ineos ABS Lustran® QE 1122, Injection Grade
(discontinued **) Injection molding grade, very high impact combined with high modulus, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEO.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm |
762 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good .. |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 60243-1 |
Lanxess Pocan® B 1600 000000 PBT PBT, non-reinforced, injection molding, extrusion, food contact |
|||
Dielectric Strength | 30.0 kV/mm | 762 kV/in | ASTM D149 |
Kuraray Genestar™ GR2300 Nylon, 30% Glass Filled Standard V-0 Grade. Delivers increased fluidity and weld strength. Well suited for a wide range of electrical and electronic components. |