Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | 120°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® K200 Standard Grade Acetal Resin Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Kolon KOCETAL® UR304 Toughened Grade Acetal Resin TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 1.00 mm |
483 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East) NORYL EN110 is an extrusion material with a Vicat B/120 of 115°C according ISO 306. NORYL EN110 is a standard extrusion grade for applications where medium temperature resistance is required.This.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Tepcon M270 Acetal-copolymer (POM), High Fluidity, High Cycle Information provided by PolyPlastics. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
Short time; ASTM D149 |
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder 25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
Gharda Chemicals Gafone S 1500 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LARTON GCE/60 60% Mixed Glass Fiber and Special Mineral Filled Polyphenylene sulfide (PPS)
(discontinued Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 19.0 kV/mm | 483 kV/in | IEC 60243-1 |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Dielectric Strength | 19.0 kV/mm @Thickness 2.00 mm |
483 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G0 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |