Polymer Property : Dielectric Strength = 4060 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 160 kV/mm

@Thickness 3.00 mm
4060 kV/in

@Thickness 0.118 in
ASTM D149
Solvay Specialty Polymers Ajediumâ„¢ Film Thermoplastic Polyimide (PI, TP)
TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra..
Dielectric Strength 160 kV/mm
4060 kV/in
K20/P50; IEC 60243-1
Styrolution Polystyrol 454 C GR 2 PS
Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 815 High Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 815 is a high heat resistant, high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stab..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 818 Easy Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which r..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 822 Standard Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 822 is a good flow, environmentally friendly high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good d..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 849 High Flow, High Heat Resistance Polystyrene
Total Petrochemicals Polystyrene 849 is a high flow, high heat resistant polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensional stabil..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 850S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 850S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene
Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 863 High Flow Flame Retardant Deca Polystyrene
Total Petrochemicals Polystyrene 863 is a high flow, heat resistant, high impact polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensiona..
Dielectric Strength 160 kV/mm
4060 kV/in
ASTM D149
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene
Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi..
Dielectric Strength 160 kV/mm
4060 kV/in
at 0.075 mm
Goodfellow Polyethylene Naphthalate (PEN) Film
A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colo..
Dielectric Strength >= 160 kV/mm
>= 4060 kV/in
CEN® Electronic Material CN Polyimide Film, 3 Mil Thickness
CEN®CN polyimide film is typical general-purpose polyimide film and has been used successfully in applications at temperatures as low as -269°C (-452°F) and as high as 400°C (752°F). CN film ca..
Dielectric Strength >= 160 kV/mm
>= 4060 kV/in
ASTM D149
CEN® Electronic Material CV Polyimide Film, 3 Mil Thickness
CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup..