Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 1200H-15 Polyester SMC Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | |
Arkema Group Oroglas® DRT Acrylic, Impact Grade
(discontinued **) For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | Short Term per ASTM D149. |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
IDI Composites A-205 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-HFk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-HL Gap Filler Pad Sarcon GR-L is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | Wet, step-by-step. ASTM D149 |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | DIN 53481 |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | JIS K2111 |
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | |
Covestro Baydur® 110 FR Polyurethane Rigid microcellular RIM polyurethane material. Fast demold times; self releasing; long flow paths possible, therefore suitable for production of large moldings. Parts are injected through only one .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | IEC 60243-1 |
DSM Stanyl® TW441 (COND) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.00 mm |
381 kV/in @Thickness 0.118 in |
step by step; IEC 60243 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm @Thickness 1.00 mm |
381 - 508 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Raschig Group 5557 DAP
(discontinued **) Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America FS-4 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Dielectric Strength | 15.0 - 100 kV/mm | 381 - 2540 kV/in | Average value: 28.1 kV/mm Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |