Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 3.94 kV/mm | 100 kV/in | Short Term; ASTM D149 |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Garlock THERMA-PURâ„¢ 4122-KAMM High Temperature Gasketing Material THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a u.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | ASTM D149 |
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum Information provided by ITW Devcon |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive TRA-BOND 2122 is a versatile aluminum metal filled epoxy formulation developed for modern industrial casting, bonding and repair applications where a strong aluminum-like adhesive is required. This .. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Dow Corning SE 4490 CV One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Cotronics Duralco™ 4540 Machinable Epoxy Patches, fills, seals, and repairs with outstanding adhesion, ductility, thermal conductivity and shock resistance.Corrosion Resistance: excellent resistance to chemicals and solventsApplications: .. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Cotronics Resbond™ 7030 High Temperature Ceramic Adhesive, High Strength |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Cotronics Resbond™ 918 High Temperature Ceramic Adhesive, One Composition |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | ASTM D149 |
Devcon HVAC Repair (Special F) Epoxy General Repair EpoxyComments: Aluminum-filled epoxy adhesive, conveniently packaged in two 6.5 oz. tubes. Bonds to aluminum and other metals, ceramics, wood, concrete or glass. Use as an adhesive .. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | 35% RH |
3M Novec™ 1710 Electronic Grade Coating 3M™ Novec™ 1710 Electronic Grade Coating is a higher solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 10 wt% fluorochemical acrylic polymer carried i.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate Good mechanical strength, and electrical and thermal resistance. For producing insulators, standoffs, feed-thrus, furnace carriers and brazing fixtures. Fabricate and fire yourself using conventio.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia Two-part, quick-set ceramic for small parts. |
|||
Dielectric Strength | >= 3.94 kV/mm | >= 100 kV/in | |
3M Scotch-Seal™ 1252 Tamper Proof Sealant 3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | ASTM D149 |
3M 4508 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | 35% RH |
3M Novec™ 1702 Electronic Grade Coating 3M™ Novec™ 1702 Electronic Grade Coating is a lower solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 0.2 wt% fluorochemical acrylic polymer carried i.. |
|||
Dielectric Strength | 3.94 - 15.7 kV/mm | 100 - 400 kV/in | Average value: 13.1 kV/mm Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 3.94 kV/mm | 100 kV/in | |
Garlock THERMA-PUR™ 4122-FC High Temperature Gasketing Material THERMa-PUR™ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a uniqu.. |