Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material

Category Metal
Manufacturer Garlock Rubber Technologies
Trade Name THERMA-PUR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock THERMA-PURâ„¢ 4122-CMG High Temperature Gasketing Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
THERMa-PURâ„¢ is a proprietary gasketing material designed for use in high temperature sealing applications. It is produced using an environmentally friendly solvent-free process and combines a unique formulation with a patent-pending core.Able to withstand high temperature, whether continuous or in thermal cycling conditionsExcellent oxidation resistanceHydrophobic and electrically insulatingEasy release from flanges4122-CMG: Corrugated Metal GasketInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0492 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 8.27 MPa
1200 psi
ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1000 °C

@Pressure 6.89 MPa
1832 °F

@Pressure 1000 psi
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 3.94 kV/mm
100 kV/in
Descriptive Properties Value Comments
Compressibility, % 34-45
ASTM F36
Creep Relaxation, % 25
ASTM F38