Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | |
Plastcom SLOVAMID 66 GF 15 GB 25 TS PA66, 15% glass fibre, 25% glass beads FeaturesPA 66 chemically reinforced with 15 % glass fibre and with the content of 25% glass beads, thermo stable. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical p.. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® F 7 Polytetrafluoroethylene (PTFE) Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low .. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | IEC 60250 |
Polyram PlusTek PA351M8 Nylon 6.6 for Injection Molding, 40% Mineral Reinforced 40% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | VDE 0303/4 |
Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled 30% low friction mineral filled polyamide 6.6 lubricated with molybdenum for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | IEC 60250 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | |
Von Roll Isola IMI Varnish 74011 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa.. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | IEC 60250 |
Polyram PlusTek PA350M6 Nylon 6.6 for Injection Molding, 30% Mineral Reinforced 30% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | |
Von Roll Isola IMI Varnish 74001 Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 24°C. Average solids: 92.5%. Usage Notes: Clear epoxy insulating varnish which penetrates and saturates extremely well, giving outstanding moisture .. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | |
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced Heat resistant grade with halogen-free flame retardant; applications include TV plug connectors and components in switchgear cabinets.Data was collected by ISO methods and provided by BASF. |
|||
Dielectric Strength | 85.0 kV/mm | 2160 kV/in | |
BASF Luranyl® KR 2454/3 G4 Polyphenylene Ether + Styrene-Butadiene Blend, 20% Glass Fiber Reinforced Glass fiber reinforced grade containing halogen-free flame-retardant; for moldings with high heat resistance and stiffness (e.g. relay parts, controller and switch housings).Data was collected by IS.. |
|||
Dielectric Strength | 85.0 - 95.0 kV/mm | 2160 - 2410 kV/in | Average value: 90.0 kV/mm Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |