Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
Ineos ABS Lustran® M305 Grade for smart cards, good dimensional accuracy, excellent dynamic loading capacity.,Property data per ISO test methods. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 243-1 |
Solvay Technyl® A 218 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243 |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 243-1 |
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0 Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Styrolution Luran® 358 N SAN Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.50 mm |
864 kV/in @Thickness 0.0591 in |
Short Time; IEC 60243-1 |
Styrolution Novodur® H802 ABS Novodur H802 is a high heat injection molding grade with high stiffness, especially suitable for being painted.Information provided by Styrolution |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60250 |
Polyram RamSter PF300G9 PBT, 45% Glass Fiber 45% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | VDE 0303/4 |
Polyram RamSter RF300G4 PBT, 20% Glass Fiber 20% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
Covestro Baygal® 90 IK 69 Polyurethane Uses: Suitable for impregnation and encapsulation of coils, especially when high heat deflection temperature, and eventually fire resistance is requested.Information provided by Bayer.As of 1 Septem.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 3156 Polycarbonate ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® LED2045 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable .. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® LQ3147 Polycarbonate ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints .. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-30 PA6-GF30 Product description: Grilon BG-30 is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 has the following important properties: High stiffnessGood balance between stre.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3X V0 nat 6059 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSGZ-30 PA666-GF30 Product description: Grilon TSGZ-30 is a heat stabilized, normal viscosity, and impact modified PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSGZ-30 has the following important p.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 3959 nat PA610 Product description: Grilamid XE 3959 natural is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materia.. |
|||
Dielectric Strength | 34.0 kV/mm @Temperature 23.0 °C |
864 kV/in @Temperature 73.4 °F |
ISO 60243-1 |
Ensinger TECASINT™ 2021 Polyimide, Brown (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce.. |
|||
Dielectric Strength | 34.0 kV/mm | 863 kV/in | ASTM D149 |
Arlon 44141R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Styrolution Luran® 368 R SAN General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |