Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Short Time; 1/8 inch; ASTM D149 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM 7040 MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6 IM 7050 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier, Nucleating Agent and LubricantFeatures: Heat Stabilized, Impact Modified, Nucleated and LubricatedInformation pro.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/66 IM 6040 MB Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® TPX-PBT-01006 40% Glass/Ceramic Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Ceramic, 40% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS 484 GY Availability: North AmericaForms: PelletsAppearance: GreyInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS LE BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 8813148Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 CM30 HS BK 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackInf.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 CM40 HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Comp.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 HS L Colors Heat Stabilized Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: Colors AvailableTPCI# 10014102Information provided by TP Composite.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 HS YL030 Heat Stabilized Availability: North AmericaForms: PelletsFeatures: Fast Molding Cycle and Good AdhesionAppearance: YellowTPCI# 10054102Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 L N MB (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability and NucleatedTPCI# 7964102Information provided by TP Co.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 L UV (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6 L N BK002 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and Lubricant(4500 ppm)Features: Fast Molding Cycle, Good Processability, Nucleated and LubricatedAppearance: BlackTPCI# 1327102In.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK MB Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Dielectric Strength | 18.1 kV/mm @Thickness 3.00 mm |
460 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® HIPS TM40 WT 40% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin.. |
|||
Dielectric Strength | 18.1 kV/mm @Thickness 3.00 mm |
460 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced Features: Good creep Resistance; Good stiffness; Good dimensional stability; High strength; Heat stabilized Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | |
Tra-Con Tra-Bond 2147 Thixotropic Epoxy/Polyamide Adhesive TRA-BOND 2147 is a thixotropic (thick paste) polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | |
Tra-Con Tra-Bond FS163 Medium Viscosity Epoxy/Polyamide Adhesive TRA-BOND FS163 is a medium viscosity polyamide/epoxy adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are r.. |
|||
Dielectric Strength | 18.1 kV/mm | 460 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PBT FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |