Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.2 kV/mm | 385 kV/in | Short Term; ASTM D149 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Dielectric Strength | 15.2 kV/mm | 385 kV/in | Short Term; ASTM D149 |
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Dielectric Strength | 15.2 kV/mm | 385 kV/in | ASTM D149 |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Dielectric Strength | >= 15.2 kV/mm @Temperature 121 °C, Time 10800 sec |
>= 385 kV/in @Temperature 250 °F, Time 3.00 hour |
0.0625 in. thickness; ASTM D149 |
Garlock MULTI-SWELLâ„¢ 3760 Compressed Aramid Fiber Gasketing Aramid fibers with a proprietary rubber binder.Creates compressive load in light weight flanges in oil and water serviceTwice as compressible as standard fiber gasketsSeals with low load and irregul.. |
|||
Dielectric Strength | 15.2 kV/mm | 386 kV/in | 60Hz, Step-by-Step, dry; ASTM D149 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 15.2 kV/mm | 386 kV/in | Short Time; ASTM D149 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Dielectric Strength | 15.2 kV/mm | 385 kV/in | |
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
Dielectric Strength | 15.2 kV/mm | 385 kV/in | |
Dow Corning SLYGARD® 527 A&B SILICONE DIELECTRIC GEL Two-parts, clear, RT or heat cure.Information provided by Dow Corning |
|||
Dielectric Strength | 15.2 kV/mm | 385 kV/in | ASTM D149 |
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Dielectric Strength | 15.2 kV/mm | 385 kV/in | |
Dow Corning 3-4150 DIELECTRIC GEL KIT Two-part, transparent green, fast RT or heat cure.Information provided by Dow Corning |
|||
Dielectric Strength | 15.2 - 16.9 kV/mm | 385 - 430 kV/in | Short Time |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Dielectric Strength | 15.2 - 16.7 kV/mm | 386 - 424 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 99 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |