Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 0.800 mm |
381 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific) Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v.. |
|||
Dielectric Strength | 15.0 - 20.0 kV/mm | 381 - 508 kV/in | IEC 60243-1 |
Raschig Group 3572 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | |
Arkema Group Oroglas® HFI-10 Acrylic, Impact Grade
(discontinued **) OROGLAS HFI-10 is an impact grade that in addition to its superior impact resistance provides an improvement in flow which contribute to improve molding behavior and reduce cycle time.Key features :.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 1.00 mm |
381 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Dielectric Strength | >= 15.0 kV/mm | >= 381 kV/in | 1 MHz |
MarkeTech AO 95 Aluminum Oxide Ceramic Substrate, 95% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 4.0 x 6.0 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
IDI Composites E-204 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Dielectric Strength | 15.0 kV/mm | 380 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PC E IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM ATX200F PEI (Europe-Africa-Middle East) High flow Polyetherimide blend. Resin is RoHS compliant. UL94 V0 Listing. US FDA Food Contact compliant. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.20 mm |
381 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |
|||
Dielectric Strength | 15.0 kV/mm @Thickness 3.00 mm |
380 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 133 GVH Nylon 66, 30% Glass Fiber Reinforced Notes: Excellent for connectors and electrical parts; Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength |
|||
Dielectric Strength | 15.0 kV/mm | 380 kV/in | |
Tra-Con Tra-Bond 2230 Color Keyed, High Temperature Epoxy Adhesive TRA-BOND 2230 is a clear, low viscosity, high temperature, two-part epoxy adhesive that changes colors during the curing process to indicate cure status. The unmixed components are light yellow; the.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | cond; IEC 60243-1 |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Dielectric Strength | 15.0 kV/mm | 380 kV/in | ASTM D149 |
Ensinger Tecanat™ Unfilled Polycarbonate (PC) Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps.. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | IEC 60112 |
Proto3000 PC Fused Deposition Modeling Polymer Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | ASTM D149 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Dielectric Strength | 15.0 kV/mm | 381 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI.. |