Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MarkeTech AO 95 Aluminum Oxide Ceramic Substrate, 95% Purity

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer MarkeTech
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech AO 95 Aluminum Oxide Ceramic Substrate, 95% Purity.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 4.0 x 6.0 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µm polished.
Physical Properties Metric English Comments
Density >= 3.65 g/cc
>= 0.132 lb/in³
Mechanical Properties Metric English Comments
Flexural Strength >= 275 MPa
>= 39900 psi
Thermal Properties Metric English Comments
CTE, linear <= 7.70 µm/m-°C

@Temperature 20.0 °C
<= 4.28 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 27.0 W/m-K
187 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
Dielectric Constant 9.2

@Frequency 1e+6 Hz
9.2

@Frequency 1e+6 Hz
Dielectric Strength >= 15.0 kV/mm
>= 381 kV/in
1 MHz
Dissipation Factor 0.00030

@Frequency 1e+6 Hz
0.00030

@Frequency 1e+6 Hz
Users viewing this material also viewed the following: