Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 12.8 kV/mm | 325 kV/in | ASTM D149 |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; Dry; ASTM D149 |
Resinoid 2002-4 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | ASTM D149 |
DSM Biomedical PurSil® AL 20 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Dielectric Strength | 12.8 - 17.0 kV/mm | 325 - 432 kV/in | Average value: 14.0 kV/mm Grade Count:13 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | ASTM D149 |
Plenco 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 204 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to accommodate a wide range of molding situations. In addition, it is recommended for use in thin wall .. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 152 Phenolic, Compression Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 22257 Phenolic, Compression Grade Durez 22257 Black Phenolic is a two-stage, asbestos-free, medium impact molding material. It is designed for appliance and electrical applications where additional mechanical strength is required. .. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 31906 Phenolic, Compression Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | 60Hz, Step-by-Step, wet; ASTM D149 |
Sumitomo Bakelite North America EM 7302 Hardware Grade Epoxy Long fiberglass reinforced epoxy molding compound which features high strength and toughness for structural components. This compound is designed for applications requiring Mil-M-46069 certificatio.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 25378 Phenolic, Compression Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; ASTM D149 |
Plenco 08225 Polyester BMC, Compression Molded PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; ASTM D149 |
Plenco 3509 Phenolic, Granular, Injection Molded PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | |
Trelleborg Emerson & Cuming Stycast® E-151-8 One-Component Epoxy Flexible Encapsulant Emerson & Cuming E-151-8 Stycast® One-Component Epoxy Flexible EncapsulantExcellent thermal shock and impact resistance. Good chemical resistance, high temperature, unfilled, low viscosity. Cure Ty.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T357 Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Dielectric Strength | 12.8 kV/mm @Frequency 60.0 Hz |
325 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America Epiall® 1908M-1 Short Glass Fiber Reinforced Epoxy Epiall 1908M-1 is a short glass fiber reinforced epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided.. |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | Short Time; Dry; ASTM D149 |
Resinoid 7201 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Dielectric Strength | 12.8 kV/mm | 325 kV/in | ASTM D149 |
Plaslok 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 204 is a two-stage, woodflour and min.. |