Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 10000 V @Temperature 90.0 - 90.0 °C |
>= 10000 V @Temperature 194 - 194 °F |
Average value: 23300 V Grade Count:8 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Breakdown | >= 10000 V @Time 20.0 - 60.0 sec |
>= 10000 V @Time 0.00556 - 0.0167 hour |
Average value: 23300 V Grade Count:8 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | Withstand Voltage [V/min]; AC 60 Hz |
Fujipoly Industries Sarcon® 85GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | Withstand Voltage [V/min]; AC 60 Hz |
Fujipoly Industries Sarcon® 85H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-Hk Gap Filler Pad Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-HL Gap Filler Pad Sarcon GR-L is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | Withstand Voltage [V/min]; AC 60 Hz |
Fujipoly Industries Sarcon® 85T Thin-Film TR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® 2042-3 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® 2283-2 Extruded PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® 2345-2 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® M787 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® M835 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® M855 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® K109 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® K350 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | |
Saint-Gobain CHR® T Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | >= 10000 V @Thickness 1.00 mm |
>= 10000 V @Thickness 0.0394 in |
|
CeramTec Rubalit® 710 Alumina, 99.6% Rubalit® 710 (99.6%) is an alumina that produces optimum results and is considered the material of choice for thin-film technology. Its characterizing features are high strength and thermal conduct.. |
|||
Dielectric Breakdown | >= 10000 V | >= 10000 V | IEC 626 |
Dr. D. Mueller Flexiso® DMD FI 14010 00240 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00240 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |
|||
Dielectric Breakdown | 10000 V | 10000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont. |
|||
Dielectric Breakdown | 10000 V | 10000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® EL Polyester Film, 300 Gauge Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 300 Gauge Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | ASTM D149 |
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge Melinex® ST580 is a clear, heat stabilized polyester film that is primed on one surface for enhanced adhesion to UV curable inks and coatings. Typical applications include flexible electronics, tou.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® WC Polyester Film, 300 Gauge Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char.. |
|||
Dielectric Breakdown | >= 10000 V | >= 10000 V | |
3M Scotch® 77 Black Fire-Retardant Electric Arc Proofing Tape Scotch® Fire-Retardant Electric Arc Proofing Tape 77 Series are designed to protect most types of electrical cables from fault arc-generated heat and flames of nearby cable failures. These elastome.. |
|||
Dielectric Breakdown | >= 10000 V | >= 10000 V | |
3M Scotch® 77 White Fire-Retardant Electric Arc Proofing Tape Scotch® Fire-Retardant Electric Arc Proofing Tape 77 Series are designed to protect most types of electrical cables from fault arc-generated heat and flames of nearby cable failures. These elastome.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | Standard condition; ASTM D1000 |
3M Scotch® Super 88 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape Super 88 is a premium grade, 8.5 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is.. |
|||
Dielectric Breakdown | 10000 V | 10000 V | ASTM D149 |
DuPont Teijin Films Melinex® ST557 Polyester Film, 200 Gauge Melinex® ST557 is a slightly hazy polyester film with low shrinkage, good flatness, and excellent handling properties. Melinex® ST557 is pretreated with a unique primer on both surfaces for adhesi.. |
|||
Dielectric Breakdown | >= 10000 V @Temperature 90.0 - 90.0 °C |
>= 10000 V @Temperature 194 - 194 °F |
Average value: 32900 V Grade Count:5 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Breakdown | >= 10000 V @Time 20.0 - 60.0 sec |
>= 10000 V @Time 0.00556 - 0.0167 hour |
Average value: 32900 V Grade Count:5 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |