Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 10.0 - 1.00e+11 ohm | 10.0 - 1.00e+11 ohm | Average value: 4.63e+9 ohm Grade Count:24 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Insulation Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | Average value: 1.94e+10 ohm Grade Count:6 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Insulation Resistance | 1.00e+8 - 1.00e+11 ohm | 1.00e+8 - 1.00e+11 ohm | Average value: 2.78e+10 ohm Grade Count:10 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Insulation Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Average value: 4.52e+10 ohm Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Insulation Resistance | 1.00e+11 - 1.00e+11 ohm @Temperature 90.0 - 90.0 °C |
1.00e+11 - 1.00e+11 ohm @Temperature 194 - 194 °F |
Average value: 1.00e+11 ohm Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Insulation Resistance | 1.00e+10 - 1.00e+11 ohm @Temperature 90.0 - 90.0 °C |
1.00e+10 - 1.00e+11 ohm @Temperature 194 - 194 °F |
Average value: 7.75e+10 ohm Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Insulation Resistance | 100 - 1.00e+11 ohm | 100 - 1.00e+11 ohm | Average value: 1.67e+10 ohm Grade Count:6 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Insulation Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 6-8438-1 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Insulation Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 6-8548 Polyamide 12, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Suitable for discharging of statically generated electricity.Dynamic stressed parts.Low waterab.. |
|||
Insulation Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | Dry; IEC 167 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Insulation Resistance | 1.00e+10 - 1.00e+11 ohm | 1.00e+10 - 1.00e+11 ohm | Dry; IEC 167 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
Insulation Resistance | 1.00e+9 - 1.00e+11 ohm | 1.00e+9 - 1.00e+11 ohm | Dry; IEC 167 |
Vyncolit X682 Novolac Phenolic Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info.. |
|||
Insulation Resistance | 10000 - 1.00e+11 ohm | 10000 - 1.00e+11 ohm | Average value: 3.33e+10 ohm Grade Count:3 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |