Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 32.0 kV/mm @Thickness 0.800 mm |
813 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 0.800 mm |
813 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 0.800 mm |
813 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East) XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
813 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
813 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
813 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |
|||
Dielectric Strength | 32.0 kV/mm @Thickness 1.00 mm, Temperature 90.0 °C |
813 kV/in @Thickness 0.0394 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |