Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.7 kV/mm @Thickness 3.17 mm |
500 kV/in @Thickness 0.125 in |
in oil; ASTM D149 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
D-48/50 |
Industrial Laminates/Norplex NP180 Synthetic Fabric
(discontinued **) Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.Thickness Tested: .. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP101 Synthetic Fabric Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP320E Cotton Fabric Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500†|
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP691 Paper Base Laminate Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0... |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.57 mm |
500 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.02 mm |
500 kV/in @Thickness 0.0400 in |
ASTM-D149 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 1.91 mm |
500 kV/in @Thickness 0.0750 in |
Silicone Rubber Insulator; ASTM D149 |
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl.. |
|||
Dielectric Strength | 19.7 kV/mm @Thickness 3.20 mm |
500 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |