Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer Polyplastics Co.
Trade Name FR-PET®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 130 MPa
18900 psi
ISO 527-1, 2
Elongation at Break 1.9 %
1.9 %
ISO 527-1, 2
Flexural Strength 210 MPa
30500 psi
ISO 178
Flexural Modulus 10.1 GPa
1460 ksi
ISO 178
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 227 °C
441 °F
ISO 75-1, 2
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
IEC 60093
Surface Resistance 5.00e+16 ohm
5.00e+16 ohm
IEC 60093
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Comparative Tracking Index 250 V
250 V
IEC 60112
Users viewing this material also viewed the following: