Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an .. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
LG Chemical LUCEL GC240 POM+GF40%, High Rigidity Feature: Injection Molding, POM+GF40%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Menzolit Menzolit® BMC 2400 Unsaturated Polyester UP BMC 2400 is a general purpose BMC for applications in the field of low smoke density and non toxic smoke.. The flammability meets the demands of EN45545 and is classified according to British standa.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry) Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | DIN 53482 |
Polyram RamTough PZ307G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced, UV stabilized polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | DIN 53482 |
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber 15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Covestro Baydur® 60 Polyurethane Rigid integral skin polyurethane foam for engineering components. The integral distribution of density gives a higher flexural modulus. If required, the property level can be improved by increasing .. |
|||
Surface Resistance | 1.00e+14 ohm @Temperature 23.0 °C |
1.00e+14 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers VESPEL TP-8212 Polyimide DuPont Vespel TP-8212 parts are specified for high-temperature applications requiring electrical insulation. TP-8212 parts offer a unique balance of mechanical and thermal properties with a low coef.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | CEI 60093 |
Addiplast Addinyl B2 R Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
BASF Novolen® 1102 G Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
BASF Novolen® 1102 H Polypropylene Grade with high processing stability for packaging tapes, film tape, fibrillated film, monofilaments, thermoformed and blow molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
BASF Polystyrol® 143 E Polystyrene (Europe) Medium strength, easy flowing general-purpose grade, suitable for blending with impact-modified Polystyrol, Styrolux and as a coextruded glossy capping layer.Data was collected by ISO methods and pr.. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
CEN® Electronic Material CV Polyimide Film, 5 Mil Thickness CEN®CV polyimide film keeps the same film properties as CEN®CN polyimide film, and has an excellent balance of physical, chemical, and electrical properties over a wide temperature range. With sup.. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Surface Resistance | >= 1.00e+14 ohm | >= 1.00e+14 ohm | ASTM D257 |
Gharda Chemicals Gafone S 1500 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU)
(Unverified Data**) Veradel 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Ineos ABS NOVODUR® P3T ABS, Injection Grade
(discontinued **) Injection molding grade, higher heat resistance.Applications: Automotive industry.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued pri.. |
|||
Surface Resistance | 1.00e+14 - 1.50e+14 ohm | 1.00e+14 - 1.50e+14 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | |
Polimeri Europa SINKRAL PD F332 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MGN,105-15-16-20 General purpose injection grade which combines excellent thermal stability during processing with.. |
|||
Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | IEC 60093 |
Polyram RamShine PAS703 ASA, UV Stabilized Is a general purpose injection molding ASA, good chemical resistance, UV stabilization.Information provided by Polyram. |