Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Surface Resistance | >= 1.00e+12 ohm | >= 1.00e+12 ohm | |
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | cond.; IEC 60093 |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | Between Layers |
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical .. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ASTM D257 |
Techmer ES Elastoblend® PA6/6 GF43 IM L 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedTPCI# 6439.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | DIN 53482 |
Polyram PlusTek PB304G7 Nylon 6, 35% Glass Fiber 35% glass-fiber reinforced, heat stabilized and impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Polyram PlusTek PB300G4 Nylon 6 for Injection Molding, 20% Glass-Fiber Reinforced 20% Glass fiber reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® 1SVX-50H nat PA1010-GF50 Product Description: Grilamid 1SVX-50H natural is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile: Raw materials based on renewable resources E.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® BFZ 3 PA6 Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties: Extreme toughnessEasy processingLow density Gril.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® L 20 G grey 9280 PA12 Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® TSG-35/4 H black 9836 PA666-GF35 Product description: Grilon TSG-35/4 H is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | |
Covestro Texin® 950 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated f.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | ISO 3915 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60 Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
Surface Resistance | <= 1.00e+12 ohm | <= 1.00e+12 ohm | DIN IEC 60093 |
BASF Neopolen® P 9230 A 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | |
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+14 ohm | 1.00e+12 - 1.00e+14 ohm | Average value: 4.68e+13 ohm Grade Count:12 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |