Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.20e+17 ohm-cm
100 - 1.20e+17 ohm-cm
Average value: 8.69e+15 ohm-cm Grade Count:110
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Electrical Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Average value: 500000 ohm-cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Electrical Resistivity 100 - 1.00e+17 ohm-cm
100 - 1.00e+17 ohm-cm
Average value: 1.27e+16 ohm-cm Grade Count:37
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 1.42e+16 ohm-cm Grade Count:81
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Electrical Resistivity 100 - 1.30e+13 ohm-cm
100 - 1.30e+13 ohm-cm
Average value: 1.00e+12 ohm-cm Grade Count:5
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 7.19e+16 ohm-cm Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Electrical Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
Average value: 117000 ohm-cm Grade Count:15
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced
Electrical Resistivity 100 ohm-cm - 1e+05
100 ohm-cm - 1e+05
ASTM C611
Techmer ES Electrafil® J-50/CF/20/TF/15 Polycarbonate, 20% Carbon Fiber Reinforced, 15% PTFE
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE
Electrical Resistivity <= 100 ohm-cm

@Temperature 1000 °C
<= 100 ohm-cm

@Temperature 1830 °F
ASTM D1829
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia
Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Electrical Resistivity 100 - 1.00e+6 ohm-cm

@Temperature 20.0 °C
100 - 1.00e+6 ohm-cm

@Temperature 68.0 °F
Acerde Silicon Carbide
Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert..
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 100 - 9.90e+9 ohm-cm
100 - 9.90e+9 ohm-cm
Average value: 6.61e+8 ohm-cm Grade Count:19
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Electrical Resistivity 100 - 1.00e+17 ohm-cm
100 - 1.00e+17 ohm-cm
Average value: 1.55e+15 ohm-cm Grade Count:122
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Electrical Resistivity 100 - 1.00e+16 ohm-cm
100 - 1.00e+16 ohm-cm
Average value: 5.17e+15 ohm-cm Grade Count:6
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded