Material Notes:
Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inertnessSilicon Carbide main applications domains: Refractories (furnace protection, nuclear, aerospace), Heating apparatus (Resistivity heaters, holders), Machining tools (cutting tools, abrasive, friction), Chemistry (catalyst holders, medical), Optics (mirrors for telescope), Crucibles (foundries), SusceptorsInformation provided by Acerde
Physical Properties Metric English Comments
Density 3.21 g/cc
0.116 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 2800
2800
Tensile Modulus 420 GPa
60900 ksi
Flexural Strength 610 MPa
88500 psi
Thermal Properties Metric English Comments
CTE, linear 4.00 - 5.00 µm/m-°C

@Temperature <=1000 °C
2.22 - 2.78 µin/in-°F

@Temperature <=1830 °F
Thermal Conductivity 63.0 - 155 W/m-K

@Temperature 20.0 °C
437 - 1080 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Melting Point 2730 °C
4950 °F
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.00e+6 ohm-cm

@Temperature 20.0 °C
100 - 1.00e+6 ohm-cm