Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00 - 1.00e+6 ohm-cm | 1.00 - 1.00e+6 ohm-cm | Average value: 270000 ohm-cm Grade Count:35 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 8.33e+14 ohm-cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | Average value: 21.1 ohm-cm Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Electrical Resistivity | 1.00 - 1.00e+7 ohm-cm | 1.00 - 1.00e+7 ohm-cm | Average value: 160000 ohm-cm Grade Count:39 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | Average value: 23.3 ohm-cm Grade Count:20 |
Overview of materials for Polycarbonate, NCG Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | ASTM D257 |
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1.00 - 1.00e+6 ohm-cm | 1.00 - 1.00e+6 ohm-cm | Average value: 143000 ohm-cm Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Electrical Resistivity | 1.00 - 2.00e+13 ohm-cm | 1.00 - 2.00e+13 ohm-cm | Average value: 1.25e+12 ohm-cm Grade Count:18 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | Average value: 21.3 ohm-cm Grade Count:6 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Electrical Resistivity | 1.00 - 1.00e+16 ohm-cm | 1.00 - 1.00e+16 ohm-cm | Average value: 1.16e+15 ohm-cm Grade Count:126 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1.00 - 1.00e+13 ohm-cm | 1.00 - 1.00e+13 ohm-cm | Average value: 4.17e+11 ohm-cm Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-3/CF/30 Nylon 6, 30% Carbon Fiber Reinforced |
|||
Electrical Resistivity | 1.00 ohm-cm | 1.00 ohm-cm | Specific Resistance |
UBE Tyranno Grade G Ceramic Semi-Conductive Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | |
A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 1.00 - 10.0 ohm-cm | 1.00 - 10.0 ohm-cm | |
A. Schulman ComAlloy E-16902N PPS Alloy, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 1.00 - 1000 ohm-cm | 1.00 - 1000 ohm-cm | ASTM D257 |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1.00 - 100 ohm-cm | 1.00 - 100 ohm-cm | Average value: 25.8 ohm-cm Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Electrical Resistivity | 1.00 - 1.00e+7 ohm-cm | 1.00 - 1.00e+7 ohm-cm | Average value: 1.11e+6 ohm-cm Grade Count:9 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |
|||
Electrical Resistivity | 1.00 - 9.90e+10 ohm-cm | 1.00 - 9.90e+10 ohm-cm | Average value: 2.22e+9 ohm-cm Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 1.00 - 1.00e+17 ohm-cm | 1.00 - 1.00e+17 ohm-cm | Average value: 2.63e+15 ohm-cm Grade Count:46 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |