Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+11 - 4.00e+16 ohm-cm | 1.00e+11 - 4.00e+16 ohm-cm | Average value: 1.05e+15 ohm-cm Grade Count:72 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 1.03e+16 ohm-cm Grade Count:25 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 6.00e+15 ohm-cm Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+16 ohm-cm | 1.00e+11 - 1.00e+16 ohm-cm | Average value: 7.78e+15 ohm-cm Grade Count:9 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 1.06e+14 ohm-cm Grade Count:11 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 6.50e+15 ohm-cm Grade Count:36 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+16 ohm-cm | 1.00e+11 - 1.00e+16 ohm-cm | Average value: 1.38e+15 ohm-cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+13 ohm-cm | 1.00e+11 - 1.00e+13 ohm-cm | Average value: 4.26e+12 ohm-cm Grade Count:15 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 9.59e+15 ohm-cm Grade Count:19 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+17 ohm-cm | 1.00e+11 - 1.00e+17 ohm-cm | Average value: 7.97e+15 ohm-cm Grade Count:40 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Electrical Resistivity | 1.00e+11 - 7.00e+13 ohm-cm | 1.00e+11 - 7.00e+13 ohm-cm | Average value: 2.67e+13 ohm-cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+16 ohm-cm @Temperature 20.0 - 500 °C |
1.00e+11 - 1.00e+16 ohm-cm @Temperature 68.0 - 932 °F |
|
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 500 °C |
1.00e+11 ohm-cm @Temperature 932 °F |
ASTM D1829 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® AMN P40 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-004Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
Chang Chun Plastic Longlite PM T308J General Purpose Phenolic Molding Compound ASTM Grade per ASTM D700 is 3.Information provided by Dowell Trading Company Ltd. |
|||
Electrical Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | |
Arkema Group Rilsan® BMN P40 D Nylon 11 (Conditioned) Designation ISO 1874-PA11-P,MR,12-003Flexible grade for injection molding. Available colors: black, natural and white. Mold release agent.Flexibility. Outstanding working properties. Easy filling of.. |
|||
Electrical Resistivity | >= 1.00e+11 ohm-cm | >= 1.00e+11 ohm-cm | DIN 53482/VDE 0303 |
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Electrical Resistivity | 1.00e+11 ohm-cm @Temperature 65.0 °C |
1.00e+11 ohm-cm @Temperature 149 °F |
Insulation Resistance During 10th day Cycling (95% Relative Humidity) |
Cytec Conathane® CE-1163 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+15 ohm-cm | 1.00e+11 - 1.00e+15 ohm-cm | Average value: 9.17e+13 ohm-cm Grade Count:12 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Electrical Resistivity | 1.00e+11 - 2.00e+15 ohm-cm | 1.00e+11 - 2.00e+15 ohm-cm | Average value: 2.79e+14 ohm-cm Grade Count:13 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+14 ohm-cm | 1.00e+11 - 1.00e+14 ohm-cm | Average value: 1.63e+13 ohm-cm Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |