Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.70 mm |
60 - 120 arcs @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
PLC 1 |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL 10 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
PLC 1 |
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
(BK) |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupox® GP2306FS PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, Anti-Hydrolysis Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chem.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupoy 1301EP22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 3.00 mm |
60 - 120 arcs @Thickness 0.118 in |
|
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
High Amp Arc Ignition, HAI | 60 - 119 arcs @Thickness 3.00 mm |
60 - 119 arcs @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |