Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.70 mm |
>= 120 arcs @Thickness 0.0669 in |
UL 746 |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
PLC 0 |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
PLC 0 |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
PLC 0 |
PTS Tristar® PC-10R-CL(6) 6 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
PLC 0 |
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
|
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
|
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
|
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
|
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
|
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.30 mm |
>= 120 arcs @Thickness 0.130 in |
|
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.30 mm |
>= 120 arcs @Thickness 0.130 in |
|
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.30 mm |
>= 120 arcs @Thickness 0.130 in |
|
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
|
LG Chemical Lupox® GP2076F PBT+GF7% Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
|
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
PLC 0 |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
PLC 0 |
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
PLC 0 |
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.60 mm |
>= 120 arcs @Thickness 0.0630 in |
PLC 0 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |