Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 1.70 mm |
60 - 120 sec @Thickness 0.0669 in |
UL 746 |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 1.70 mm |
60 - 120 sec @Thickness 0.0669 in |
UL 746 |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 3.00 mm |
60 - 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 0.400 mm |
60 - 120 sec @Thickness 0.0157 in |
PLC 1; UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 1.50 mm |
60 - 120 sec @Thickness 0.0591 in |
(ALL) |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 1.50 mm |
60 - 120 sec @Thickness 0.0591 in |
(BK, BN) |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 0.840 mm |
60 - 120 sec @Thickness 0.0331 in |
BK |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301EP22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000HU PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: Electric & Electronic (Housing, Components) For Suit caseCAS: 103598-77-2Information provided by LG Chemic.. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000LS PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, Electric & Electronic Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided .. |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness >=3.00 mm |
60 - 120 sec @Thickness >=0.118 in |
|
LG Chemical LUPOY GP1000SW PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 60 - 120 sec @Thickness 2.40 mm |
60 - 120 sec @Thickness 0.0945 in |
UL 746 |
Teknor Apex APEX® 92-A2292C-90 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: Flame Retardant; High Heat Resistance Uses: Cable JacketingForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54.. |