Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 349 - 400 °C | 660 - 752 °F | Average value: 380 °C Grade Count:32 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Melt Temperature | 349 - 400 °C | 660 - 752 °F | Average value: 376 °C Grade Count:9 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Melt Temperature | 380 - 400 °C | 716 - 752 °F | |
LATI LARPEEK 50 G/40 40% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 380 - 400 °C | 716 - 752 °F | |
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 380 - 400 °C | 716 - 752 °F | |
LATI LARPEEK 50 K/30 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 330 - 400 °C | 626 - 752 °F | Average value: 364 °C Grade Count:8 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 390 - 400 °C | 734 - 752 °F | |
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Melt Temperature | 380 - 400 °C | 716 - 752 °F | |
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced High thermal conductivity product based on Polyetheretherketone (PEEK). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 380 - 400 °C | 716 - 752 °F | |
LATI Latigray 88/10-01 CX/30 PEEK Radiopaque compound based on Polyetheretherketone (PEEK). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 380 - 400 °C | 716 - 752 °F | |
LATI LARPEEK 50 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Melt Temperature | 370 - 400 °C | 698 - 752 °F | |
LATI Latilub 88/50-20GRT K/10 PEEK, 10% Carbon Fiber Reinforced, Graphite/PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid.. |