Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Temperature | 299 - 330 °C | 570 - 626 °F | Average value: 308 °C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA), 25% GlassCarbon Fiber Amodel® A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer .. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V215A 15% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V220A 20% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V235A 35% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V240A 40% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | Injection-molding/Extrusion |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | Injection-molding/Extrusion |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | Injection-molding/Extrusion |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Conditioned) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | Injection-molding/Extrusion |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | Injection molding/Extrusion |
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned) Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V250A 50% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® V330FR 30% Glass Fiber Reinforced Flame Retardant PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Melt Temperature | 310 - 330 °C | 590 - 626 °F | |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled Self-lubricating product based on Polysulfone (PSU). Graphite. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Melt Temperature | 300 - 330 °C | 572 - 626 °F | |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |
|||
Melt Temperature | 320 - 330 °C | 608 - 626 °F | DAM |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)