Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 304 - 327 °C | 580 - 620 °F | |
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristics: High Str.. |
|||
Melt Temperature | 270 - 327 °C | 518 - 620 °F | Average value: 303 °C Grade Count:45 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Melt Temperature | 282 - 327 °C | 540 - 620 °F | Average value: 304 °C Grade Count:5 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Melt Temperature | 316 - 327 °C | 600 - 620 °F | Molding |
PolyOne Edgetek® SF-30GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 327 °C | 600 - 620 °F | Molding |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Temperature | 299 - 327 °C | 570 - 620 °F | |
Chevron Phillips MarFlex® 1023 LDPE Extrusion Coating Resin Resin Type: Base, SpeedCharacteristics: Good adhesion at low coating weights and high line speedsLow COF usesFDA approved for food contactApplications: Can be used in the outer coextrusion layer or .. |
|||
Melt Temperature | 149 - 327 °C | 300 - 620 °F | Average value: 214 °C Grade Count:42 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |
|||
Melt Temperature | 293 - 327 °C | 560 - 620 °F | Molding |
PolyOne Lubri-Tech™ MP-20CF/15T Modified Polyphenylene Oxide (mPPO), Carbon Fiber Reinforced, PTFE Lubricated
  Description/Features:Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 304 - 327 °C | 580 - 620 °F | Molding |
PolyOne Edgetek® AM-10CF-20GF/000 HS Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |