Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Gravi-Tech™ GRV-NY-027-SS-BLK-F Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 266 - 293 °C | 511 - 559 °F | |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Gravi-Tech™ GRV-NY-050-CU-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Nymax™ GF 924 33 UV Black 108 Polyamide 66 (Nylon 66) Property data for molded test bars: Dry as MoldedInformation provided by PolyOne |
|||
Melt Temperature | 260 - 293 °C | 500 - 559 °F | |
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | |
PolyOne Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
Styron EMERGEâ„¢ 4510-15 Polycarbonate EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Inform.. |
|||
Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
Styron EMERGEâ„¢ 4530-15 Polycarbonate EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
Eastman Eastar MN058 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra.. |
|||
Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
Eastman Eastar MN059 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra.. |
|||
Melt Temperature | 277 - 293 °C | 531 - 559 °F | |
Eastman Eastar EN059 Copolyester, Natural Applications:Cosmetics/personal care packagingDeodorant PackagingFragrance packagingOral hygienePlastics for hygiene feminine productsToothbrushesToys/Sporting goodsWriting instrumentsProduct Descri.. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NL-45GF/000 Nylon 6/12 - 45% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 271 - 293 °C | 520 - 559 °F | Stock |
PolyOne Edgetek® NI-40GF/000 Nylon 6/10 - 40% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 260 - 293 °C | 500 - 559 °F | |
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |