Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 437 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 225 - 250 °C
437 - 482 °F
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
Melt Temperature 225 - 235 °C
437 - 455 °F
Blow Molding
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo..
Melt Temperature 225 - 235 °C
437 - 455 °F
Extrusion
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo..
Melt Temperature 225 - 240 °C
437 - 464 °F
Eastman Tenite 371A-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Melt Temperature 225 - 310 °C
437 - 590 °F
Average value: 269 °C Grade Count:6
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Melt Temperature 225 °C
437 °F
LCL-PR29
Intercontinental Polymers HoPBT 310 HoPBT Polymer Type - Semi-Dull, Polyester Pellets
Applications: Filament YarnInformation provided by Intercontinental Polymers.
Melt Temperature 225 °C
437 °F
LCL-PR29
Intercontinental Polymers HoPBT 545 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
Melt Temperature 225 °C
437 °F
LCL-PR29
Intercontinental Polymers HoPBT 550 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
Melt Temperature 225 °C
437 °F
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film
Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o..
Melt Temperature 225 °C
437 °F
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l...
Melt Temperature 225 - 235 °C
437 - 455 °F
Borealis Borcoat™ BB700E-7032 Polypropylene Compound for Steel Pipe Coating Applications
Borcoat BB700E-7032 is a grey colored high impact polypropylene. This product is especially designed for direct extrusion of syntactic PP with high thermal insulations capacity and high compression..
Melt Temperature <= 225 °C
<= 437 °F
Tipco Tipwood® 50 EX 50EX
Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen..
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen HU 70E3 HDPE, Injection Molding
Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding
Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen MF008S PP, 40% Glass Fiber Filled, Injection Molded
Starpylen MF008S is a 40% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen MH0200A HDPE, Injection Molding
Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding
Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen MZ006S PP, Glass Fiber Filled, Injection Molded
Starpylen MZ006S is a Glass fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WT 30GF S3)Information provided by Eurostar.
Melt Temperature 225 - 245 °C
437 - 473 °F
BASF Ultramid® HFX 37 PA6 (Dry)
Description: Ultramid HFX 37 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..
Melt Temperature 225 - 280 °C
437 - 536 °F
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 245 °C
437 - 473 °F
Beijing Ranger Chem PBT 403 M-G0 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 250 °C
437 - 482 °F
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 250 °C
437 - 482 °F
Beijing Ranger Chem PBT 403 M-G30 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 245 °C
437 - 473 °F
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 245 °C
437 - 473 °F
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 250 °C
437 - 482 °F
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 - 250 °C
437 - 482 °F
Beijing Ranger Chem PBT-MFC-G20 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Melt Temperature 225 °C
437 °F
Extrusion Coating
Braskem CN8092 EVA Molding Copolymer
CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i..
Copyright © lookpolymers.com All Rights Reserved