Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 166 - 210 °C | 330 - 410 °F | Average value: 188 °C Grade Count:4 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8915-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8940-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8950-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8980-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 8999-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9600-80 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9604-80 Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9915-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9925-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9960-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9980-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9999-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 °C | 330 °F | |
Spartech E65070 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3210-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3311-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Melt Temperature | 166 °C | 330 °F | Processing Temperature |
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Teknor Apex APEX® 3211-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8644 Moldings & Extrusions Flexible PVC General purpose extrusion compound. Forms a good bond with rigid PVC in co-extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 2134N Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness) and 94 V-0 in black and white (1.5 mm min. thickness). UL QMFZ2 recognized component.Informati.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 7810 Moldings & Extrusions Flexible PVC 105°C rated injection molding compound approved for 94 V-0 in black and white at 0.75 mm and also approved for 94 V-0 in all colors at 1.5 mm.Information provided by Georgia GulfGeorgia Gulf became.. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8542 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 8603 Moldings & Extrusions Flexible PVC A soft extrusion compound with rubber-like properties and oil resistance. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf becam.. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melt Temperature | 166 °C | 330 °F | |
Axiall 6651 Moldings & Extrusions Flexible PVC A clear molding and extrusion compound with good processing characteristics and good low temperature properties. Formulated to be resistant to fungal and microbial attack.Information provided by Ge.. |
|||
Melt Temperature | 166 - 177 °C | 330 - 350 °F | |
Sylvin Technologies 9812A-80 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 204 °C | 330 - 400 °F | |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |