Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJLF112L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 163 - 204 °C | 325 - 399 °F | |
PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
S&E Specialty Polymers TufTech™ GA-92-129 Clear PVC Compound Application: A clear, PVC-based compound designed for speaker wire applications.Information provided by S&E Specialty Polymers |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Flexible B6000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Melt Temperature | 163 - 168 °C | 325 - 334 °F | |
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 163 - 177 °C | 325 - 351 °F | |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8600-75 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8915-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8925-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8940-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8950-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8960-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8980-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 8999-75 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9077-75 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9915-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9940-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9960-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9980-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 - 174 °C | 325 - 345 °F | |
Sylvin Technologies 9999-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 163 °C | 325 °F | |
Axiall 8540 Moldings & Extrusions Flexible PVC General purpose, flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |