Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 354 - 371 °C | 669 - 700 °F | |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Melt Temperature | 20.0 - 371 °C | 68.0 - 700 °F | Average value: 184 °C Grade Count:16 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Melt Temperature | 338 - 371 °C | 640 - 700 °F | Stock |
PolyOne Stat-Tech™ PI-10SS/000 Polyetherimide - 10% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 332 - 371 °C | 630 - 700 °F | Molding |
PolyOne Edgetek® PF-30GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 371 °C | 601 - 700 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
(Unverified Data**) Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous .. |
|||
Melt Temperature | 360 - 371 °C | 680 - 700 °F | |
LNP Lubricomp® GFL-4034 EM M Polysulfone, Milled Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)& Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Melt Temperature | 316 - 371 °C | 601 - 700 °F | |
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU) Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of.. |
|||
Melt Temperature | 343 - 371 °C | 650 - 700 °F | Molding |
PolyOne Edgetek® PI-20GM/000 L Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedHigh FlowPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 354 - 371 °C | 670 - 700 °F | Molding |
PolyOne Edgetek® ES-10GF/000 PES (Polyethersulfone), 10% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Melt Temperature | 354 - 371 °C | 669 - 700 °F | |
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Melt Temperature | 354 - 371 °C | 669 - 700 °F | |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Melt Temperature | 354 - 371 °C | 669 - 700 °F | |
LNP Thermocomp® JF-1008 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |