Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0650-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1104L-xx61FRD Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information p.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1250L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX207L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 143 - 171 °C | 289 - 340 °F | |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG30BK Copolymer PP, 30% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCG40BK Copolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCM10BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCM15BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled Information provided by Niche Polymer |
|||
Melt Temperature | 149 - 171 °C | 300 - 340 °F | ASTM D789 |
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled Information provided by Niche Polymer |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Flexible B8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
PolyOne Geon™ Vinyl Flexible R881C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8600-70 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8915-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8940-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8950-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8960-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8980-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 8999-70 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9077-70 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9915-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9925-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9950-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9960-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9999-70 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 160 - 171 °C | 320 - 340 °F | |
Sylvin Technologies 9812A-70 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 166 - 171 °C | 331 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |