Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Talc Filler
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 20.0 %
20.0 %
ASTM D638
Flexural Strength 35.9 MPa
5200 psi
ASTM D790
Flexural Modulus 1.65 GPa
240 ksi
ASTM D790
Izod Impact, Unnotched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 149 - 171 °C
300 - 340 °F
ASTM D789
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: