Polymer Property : Melt Temperature = 150 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 150 - 227 °C
302 - 441 °F
Average value: 191 °C Grade Count:79
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Melt Temperature 150 - 221 °C
302 - 430 °F
Average value: 194 °C Grade Count:52
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
Stellarchem 8075 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem FP-860 TPE Compound
Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly..
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Extrusion
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
Stellarchem GP-915UB TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
Stellarchem GP-930 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem GP-9401 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem GP-9401 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem GP-965B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem GP-965B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem GP-975 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem GP-975 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Extrusion
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Injection Molding
Stellarchem GP-980 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem LP-845 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 200 °C
302 - 392 °F
Extrusion
Stellarchem MP-845B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 230 °C
302 - 446 °F
Extrusion
Stellarchem MP-950NC TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 180 °C
302 - 356 °F
Extrusion
Stellarchem SV-B40D TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Melt Temperature 150 - 180 °C
302 - 356 °F
Extrusion
Stellarchem SV-B65E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Melt Temperature 150 - 180 °C
302 - 356 °F
Extrusion
Stellarchem SV-B70E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Melt Temperature 150 - 180 °C
302 - 356 °F
Extrusion
Stellarchem SV-B80E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Melt Temperature 150 - 230 °C
302 - 446 °F
Injection Molding
Stellarchem 475-845N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Melt Temperature 150 - 180 °C
302 - 356 °F
Borealis FA6224 Low Density Polyethylene
FA6224 is a Low Density Polyethylene for Film Extrusion. Autoclave Technology. Contains Antioxidant, Anti-block and Medium Slip additives. This grade is developed for the production of thin blown f..
Melt Temperature 150 - 190 °C
302 - 374 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Melt Temperature 150 - 249 °C
302 - 480 °F
Average value: 218 °C Grade Count:5
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Melt Temperature 150 - 160 °C
302 - 320 °F
Huntsman PE8020 Specialty Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1..