Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 2.00 - 8.00 min | 2.00 - 8.00 min | |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Gel Time | 2.00 - 8.00 min | 2.00 - 8.00 min | |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, G30-700 Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Gel Time | 2.00 - 8.00 min | 2.00 - 8.00 min | |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Gel Time | 2.00 - 6.00 min | 2.00 - 6.00 min | |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Gel Time | 2.00 - 6.00 min | 2.00 - 6.00 min | |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Gel Time | 2.00 - 6.00 min | 2.00 - 6.00 min | |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Gel Time | 2.00 - 6.00 min @Temperature 135 °C |
2.00 - 6.00 min @Temperature 275 °F |
|
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Gel Time | 2.00 - 6.00 min @Temperature 135 °C |
2.00 - 6.00 min @Temperature 275 °F |
|
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 34-700 12K 2x2 Twill Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Gel Time | 2.00 - 6.00 min @Temperature 135 °C |
2.00 - 6.00 min @Temperature 275 °F |
|
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K 2x2 Twill Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Gel Time | 2.00 - 6.00 min @Temperature 135 °C |
2.00 - 6.00 min @Temperature 275 °F |
|
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Gel Time | 2.00 min | 2.00 min | |
Northstar Polymers MSB-D60A High Performance Polyurethane Cast Elastomer System This is an Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires some lord bearing, high tensile strength, cut/tear res.. |
|||
Gel Time | 2.00 - 9.00 min @Temperature 177 °C |
2.00 - 9.00 min @Temperature 351 °F |
|
Hexcel® HexPly® F263 Epoxy Resin HexPly® F263 is a structural, heat resistant epoxy resin formulated for excellent translation of high modulus carbon fiber properties in typically aerospace applications. HexPly® F263 is a high te.. |
|||
Gel Time | <= 2.00 min @Temperature 135 °C |
<= 2.00 min @Temperature 275 °F |
6 |
Hexcel® HexPly® F515 Epoxy Resin HexPly® F515 is an advanced, industrial grade, modified epoxy formulation designed for either vacuum bag or autoclave curing to offer very high laminate strengths, coupled with increased fracture t.. |
|||
Gel Time | 2.00 min | 2.00 min | |
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala.. |
|||
Gel Time | 2.00 min | 2.00 min | Slow |
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe.. |
|||
Gel Time | 2.00 min | 2.00 min | Medium |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Gel Time | 2.00 min @Temperature 93.0 °C |
2.00 min @Temperature 199 °F |
10 g |
Abatron AboCast 8110-5/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Gel Time | 2.00 min | 2.00 min | 2:1 |
ACC EP JS EPI Engineered Polymers Joint Sealant EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to prot.. |