Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced

Category Polymer , Thermoset , Epoxy
Manufacturer Park Electrochemical Corp.
Trade Name Nelcote®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K PW Carbon Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attractive finish.Key Features and Benefits:Good low pressure consolidationExcellent handling characteristics and out-timeClear surface finish for excellent cosmetic appearance on finished parts250°F cure epoxy systemApplications/Qualifications:Industrial ApplicationsRecreational ApplicationsInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Volatiles <= 1.5 %

@Temperature 135 °C
<= 1.5 %

@Temperature 275 °F
8 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 676 MPa

@Temperature 23.9 °C
98000 psi

@Temperature 75.0 °F
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D638
Tensile Modulus 62.1 GPa

@Temperature 23.9 °C
9000 ksi

@Temperature 75.0 °F
0° Direction, Dry; Oven Cure 250°F, 90 min; ASTM D3039
Flexural Strength 924 MPa

@Temperature 23.9 °C
134000 psi

@Temperature 75.0 °F
Dry; Oven Cure 250°F, 90 min; ASTM D790
Flexural Modulus 60.7 GPa

@Temperature 23.9 °C
8800 ksi

@Temperature 75.0 °F
Dry; Oven Cure 250°F, 90 min; ASTM D790
Compressive Strength 579 MPa

@Temperature 23.9 °C
84000 psi

@Temperature 75.0 °F
Dry; Oven Cure 250°F, 90 min; ASTM D695
Compressive Modulus 61.4 GPa

@Temperature 23.9 °C
8900 ksi

@Temperature 75.0 °F
Dry; Oven Cure 250°F, 90 min; ASTM D695
Shear Strength 63.4 MPa

@Temperature 23.9 °C
9200 psi

@Temperature 75.0 °F
Short-Beam, Dry; Oven Cure 250°F, 90 min; ASTM D2344
Processing Properties Metric English Comments
Gel Time 2.00 - 6.00 min
2.00 - 6.00 min
Shelf Life 6.00 Month

@Temperature -17.8 °C
6.00 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Prepreg Resin Content (%) 38-44
Resin Flow (%) 5-15
275°F, 15psi