ACC EP JS EPI Engineered Polymers Joint Sealant

Category Polymer , Thermoset
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC EP JS EPI Engineered Polymers Joint Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EP JS Joint Sealant JS, “Powered by Reactamine® Technology” is a two component 100% solid (silicone optional) polyurea based joint sealant. EP JS is a self-leveling joint sealant designed to protect interior horizontal concrete expansion and control joints from spalling, chipping, and breakdown. This elastomer displays fast cure times and excellent adhesion to concrete. EP JS can be applied at temperatures ranging -30° F to 350°F. This polyurea elastomer displays excellent chemical resistance, water insensitivity, and thermal stability at high and low temperatures. EP JS may also be used under traditional floor coatings (such as epoxies, polyureas and polyurethanes) or tiles to smooth the joints and provide protection from cracking and sinking caused by non-elastomeric joint sealants. Applications:EP JS was designed to protect against the abuse to concrete joints caused by heavy load transfers from such items as forklifts, steel-wheeled carts and trash dumpsters. Some typical uses include: Concrete Control / Expansion Joints Concrete Spall Repairs Cold Storage Facilities Merchandise Distribution Centers Home Improvement Stores Bridge Headers Warehouse Floors D.O.T. Pothole Road Repair U.S.D.A. and F.D.A. AcceptablePart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Viscosity 0.12 cP
0.12 cP
1:1, Side B
0.18 cP
0.18 cP
1:1, Side A
400 cP
400 cP
2:1, A Side
1200 cP
1200 cP
2:1, B Side
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
1:1; ASTM D2240
95
95
2:1; ASTM D2240
Tensile Strength, Yield 10.3 MPa
1500 psi
1:1; ASTM D412
20.3 MPa
2950 psi
2:1; ASTM D412
Elongation at Break 350 %
350 %
2:1; ASTM D412
800 %
800 %
1:1; ASTM D412
100% Modulus 0.00965 GPa
1.40 ksi
1:1; ASTM D412
0.0112 GPa
1.62 ksi
2:1; ASTM D412
Adhesive Bond Strength >= 2.76 MPa
>= 400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
Tear Strength 78.9 kN/m
450 pli
1:1; ASTM D412
87.7 kN/m
500 pli
2:1; ASTM D412
Taber Abrasion, mg/1000 Cycles 20.5
20.5
1:1 CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
25
25
2:1 CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
2:1 and 1:1, ASTM Pensky-Martin
Processing Properties Metric English Comments
Cure Time >= 5.00 min
>= 0.0833 hour
Tack Free Time, 2:1
>= 10.0 min
>= 0.167 hour
Tack Free Time, 1:1
Gel Time 2.00 min
2.00 min
2:1
5.00 min
5.00 min
1:1
Descriptive Properties Value Comments
Color Black, Gray
Flexibility Pass
2:1 and 1:1, ASTM D1737, 1/8"Mandrel
Resistance to Acetic Acid (100%) Recommended
Resistance to Clorox® (10%) H2O Conditional, Discoloration
Resistance to Diesel Fuel Recommended
Resistance to Gasoline Recommended
Resistance to H2O Recommended
Resistance to Hydraulic Fluid (oil) Recommended, Discoloration
Resistance to Hydrochloric Acid (20%) Recommended
Resistance to Hydrofluoric Acid(10%) Recommended, Discoloration
Resistance to Mineral Spirits Recommended
Resistance to Motor Oil Recommended, Discoloration
Resistance to Muriatic Acid (10%) Recommended
Resistance to NaCl/H2O (10%) Recommended
Resistance to Potassium Hydroxide (10%) Recommended
Resistance to Sodium Bicarbonate Recommended
Resistance to Sodium Hydroxide (10%) Recommended
Resistance to Sugar/H2O Recommended
Resistance to Sulfuric Acid (>22%) Not Recommended
Resistance to Sulfuric Acid (10%) Recommended, Discoloration
Resistance to Vinegar/ H2O (5%) Recommended
Resistance to Xylene Conditional