Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sika Industry SikaFlex 201 Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Sika Industry
Trade Name SikaFlex
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Sika Industry SikaFlex 201 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Sika 201 SikaFlex AdhesiveSikaflex 201 meets Federal Specification TT-S-00230C, Type II, Class A and ASTK C-920, Type S, Grade NS. 15 - 15 mm Cut-Off. Good non-sag. Available in black, white, gray, tan, MB bronze. Cure Type: Moisture
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0446 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 45
40 - 45
Tensile Strength, Ultimate 1.38 MPa
200 psi
Elongation at Break >= 700 %
>= 700 %
Adhesive Bond Strength 0.827 MPa
120 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 87.8 °C
190 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 240 - 480 min
4.00 - 8.00 hour
Tack-free
1440 min
24.0 hour
Value given per 1/8 inches
Shelf Life 12.0 Month
12.0 Month