Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 1.50 - 1440 min | 0.0250 - 24.0 hour | Average value: 372 min Grade Count:32 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Cure Time | 0.750 - 1440 min @Temperature 40.0 - 302 °C |
0.0125 - 24.0 hour @Temperature 104 - 576 °F |
Average value: 81.6 min Grade Count:121 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Cure Time | 1080 - 1440 min @Temperature 25.0 °C |
18.0 - 24.0 hour @Temperature 77.0 °F |
|
Fibre Glast 1099 Room Temperature Epoxy Surface Coat Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that c.. |
|||
Cure Time | 720 - 1440 min @Temperature 204 - 232 °C |
12.0 - 24.0 hour @Temperature 399 - 450 °F |
Post cure |
Lord Adhesives Chemlok® 5150 Adhesive LORD Chemlok® 5150 adhesive is a solvent-based adhesive used to bond uncured fluoroelastomers to metal. It can also be used to bond fluoroelastomers with an incorporated cure system to mechanical.. |
|||
Cure Time | 1080 - 1440 min @Temperature 23.9 °C |
18.0 - 24.0 hour @Temperature 75.0 °F |
85% maximum strength developed within |
Master Bond EP21TDCNFL Two Component Nickel Conductive Epoxy Adhesive Master Bond Polymer System EP21TDCNFL is a two component, nickel filled, electrically conductive system for high performance bonding and sealing formulated to cure at room temperature or more rapidl.. |
|||
Cure Time | 1080 - 1440 min | 18.0 - 24.0 hour | 85% of maximum strength developed |
Master Bond EP77M-1 Fast Setting, Silver Conductive Epoxy Description: Master Bond Polymer System EP77M-1 is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or.. |
|||
Cure Time | 720 - 1440 min @Temperature 23.0 °C |
12.0 - 24.0 hour @Temperature 73.4 °F |
|
Master Bond Mastersil 410 One Component Room Temperature Curing Silicon Master Bond MasterSil 410 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This compound has a pas.. |
|||
Cure Time | 720 - 1440 min @Temperature 23.0 °C |
12.0 - 24.0 hour @Temperature 73.4 °F |
|
Master Bond Mastersil 415 One Component Room Temperature Curing, Transparent Silicon Master Bond MasterSil 415 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing and protective coatings featuring high transparency. It has a paste consi.. |
|||
Cure Time | 720 - 1440 min @Temperature 23.0 °C |
12.0 - 24.0 hour @Temperature 73.4 °F |
|
Master Bond X17 Elastomer Based One Component Adhesive and Primer Master Bond Polymer System X17 is a specially formulated one component adhesive especially designed for bonding polyolefins such as polypropylene, polyethylene as well as their many co-polymers and .. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full Cure Time @ 20ºC |
Loctite® 3873 1 component acrylic High Conductivity Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Cure Time | 5.00 - 1440 min | 0.0833 - 24.0 hour | Full Cure |
Loctite® 5205 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom.. |
|||
Cure Time | 60.0 - 1440 min | 1.00 - 24.0 hour | Full Cure, Unprimed |
Loctite® 5205 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom.. |
|||
Cure Time | 60.0 - 1440 min | 1.00 - 24.0 hour | Full Cure, Unprimed |
Loctite® 5206 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5206 Flexible Cure Flange SealantSlow curing allows for micro-movement during assembly operations. Good sealing properties against oil and water/glycol. High viscosity... |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full Cure; Unprimed |
Loctite® Gasket Eliminator® 518 Flange Sealant Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can.. |
|||
Cure Time | 180 - 1440 min @Temperature 22.0 °C |
3.00 - 24.0 hour @Temperature 71.6 °F |
|
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning |
|||
Cure Time | 960 - 1440 min @Temperature 93.3 °C |
16.0 - 24.0 hour @Temperature 200 °F |
|
Cotronics Duralco™ 132 500°F (260°C) Aluminum Filled Epoxy Aluminum filled epoxy that cures at room temperature to form machinable, thermally conductive bond lines. High heat transfer. Can be supplied as a “non-sag” putty.Applications: heat tacking, hea.. |
|||
Cure Time | 960 - 1440 min | 16.0 - 24.0 hour | |
Dow BETAMATE™ 7000/7050 L Epoxy Two component room temperature fast curing polyurethane structural adhesive with high elastic modulus.Information provided by Dow |
|||
Cure Time | 960 - 1440 min @Temperature 93.3 °C |
16.0 - 24.0 hour @Temperature 200 °F |
|
Cotronics Duralco™ 122 500°F (260°C) Nickel Filled Adhesive and Casting Epoxy Specially formulated to provide an economical alternative to silver filled electrically conductive epoxies. Applications: for use in applications where highest electrically conductivity not required.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full Cure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full Cure |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP825 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP825 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Cure Time | 480 - 1440 min | 8.00 - 24.0 hour | Average value: 880 min Grade Count:3 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Cure Time | 30.0 - 1440 min | 0.500 - 24.0 hour | Full Cure |
Loctite® 5182 Flexible Cure Anaerobic Sealant Anaerobic GasketingLoctite® 5182 Flexible Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Robotic application on flanges, seals, covers |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full Cure, Unprimed |
Loctite® 5182 Flexible Cure Anaerobic Sealant Anaerobic GasketingLoctite® 5182 Flexible Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Robotic application on flanges, seals, covers |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full Cure; Unprimed |
Loctite® Gasket Eliminator® 510 Flange Sealant Anaerobic GasketingLoctite® 510 High Temperature Rigid Cure Gasket Eliminator® Flange SealantProduct has a temperature range to 400ºF with excellent solvent and chemical resistance. Makes or dre.. |