Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 240 min | 4.00 hour | On steel (fixture) |
ND Industries 420 Instant High Pressure Pipe Sealant Industrial grade, controlled locking strength for metal fittings |
|||
Cure Time | 240 min @Temperature 93.3 °C |
4.00 hour @Temperature 200 °F |
98% cure |
Reltek BONDiT™ B-46 Adhesive, Sealant & Coating System Key Properties: Excellent adhesion to low surface energy plastics without primer or surface preparation.Applications: Very high flexibility, 500% elongation, emphasizing high tack for un-abraded sub.. |
|||
Cure Time | 240 min | 4.00 hour | Full cure |
Resinlab® CYNERGY CA6310 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Cure Time | 240 - 360 min @Temperature 23.0 °C |
4.00 - 6.00 hour @Temperature 73.4 °F |
|
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast.. |
|||
Cure Time | 240 min @Temperature 150 °C |
4.00 hour @Temperature 302 °F |
Post |
Shin-Etsu Silicones KE-5006BU Low Temperature Silicone Elastomer ShinEtsu KE5006B U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-9510U Silicone Elastomer KE9510 U is one of a series of easy processing, general purpose silicone rubber base with low volatile content. It can be used in a variety of applications requiring finishing by molding, extruding .. |
|||
Cure Time | 240 min @Temperature 205 °C |
4.00 hour @Temperature 401 °F |
Post |
Shin-Etsu Silicones KE-961U Silicone Elastomer KE961 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).Pr.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-9710U Silicone Elastomer KE9710 U is one of a series of easy processing, general purpose silicone rubber base with low volatile content. It can be used in a variety of applications requiring finishing by molding, extruding .. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-971U Silicone Elastomer KE971 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).Pr.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones SF-11500U Fluorosilicone Elastomer SF11500U is a low Durometer and low modulus fluorosilicone with excellent processing ability.. Typical Applications: GasketsSealsInformation Provided by Shin-Etsu Silicones of America, Inc. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-5550U Low Temperature Silicone Elastomer ShinEtsu KE5550 U is a nominal 50 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Cure Time | 240 min @Temperature 200 °C |
4.00 hour @Temperature 392 °F |
Post |
Shin-Etsu Silicones KE-7022U Temperature Resistant Silicone Elastomer KE7022 U is intended for applications where excellent high heat resistance is required.Product Features: This product is intended for high temperature service as 55 ~+ 300 °C(67 ~ +570 °F).Typ.. |
|||
Cure Time | >= 240 min | >= 4.00 hour | |
Trelleborg Emerson & Cuming Stycast® 2651-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full Cure Time @ 20ºC |
Loctite® Output™ 315 Acrylic Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Cure Time | 240 min | 4.00 hour | Tack-Free Time |
3M AC-240 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Cure Time | 240 min | 4.00 hour | Tack-Free Time |
3M AC-251 Black Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-251 Black Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate ai.. |
|||
Cure Time | 240 min | 4.00 hour | Tack-Free Time |
3M AC-251 Gray Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-251 Gray Class B are two-part, quick curing, polysulfide based canopy and windshield sealants. These products are formulated for sealing acrylic, glass, and polycarbonate air.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT 140 |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with QM CAT PURPLE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Cure Time | 240 - 1440 min | 4.00 - 24.0 hour | Full cure |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Cure Time | 240 - 360 min | 4.00 - 6.00 hour | Tack Free Time, catalyzed with Moldmaster Green |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |