Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 50.0 - 100 MPa | 7250 - 14500 psi | |
PolyOne Bergamid™ A700 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Back Pressure | 50.0 - 150 MPa | 7250 - 21800 psi | |
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Back Pressure | >= 50.0 MPa | >= 7250 psi | Injection |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Back Pressure | >= 50.0 MPa | >= 7250 psi | Injection |
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Back Pressure | 50.0 MPa | 7250 psi | Injection |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Back Pressure | 50.0 MPa | 7250 psi | |
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Back Pressure | 50.0 - 70.0 MPa | 7250 - 10200 psi | Molding Pressure |
Azoty Tarnow™ TARFLEN SM-B40 PTFE Reinforced with 40% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Back Pressure | 50.0 - 70.0 MPa | 7250 - 10200 psi | Molding Pressure |
Azoty Tarnow™ TARFLEN SM-S25 PTFE Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |