Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 87.8 - 98.9 °C | 190 - 210 °F | |
Polymer Resources PC/ASA-GP2 Polycarbonate/ASA Alloy Acrylonitrile Styrene Acrylate + PolycarbonatePreliminary DataProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Drying Temperature | 93.3 - 98.9 °C | 200 - 210 °F | |
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Drying Temperature | 87.8 - 98.9 °C | 190 - 210 °F | 12 hours maximum |
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Drying Temperature | 82.0 - 99.0 °C | 180 - 210 °F | |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ABS/PC 7901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ABS/PC 9901 Description: Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ABS/PC FC-30 Description: Injection Molding Grade, High Impact, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ASA/PC FA-30 Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ABS/PC 8901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 93.3 - 98.9 °C | 200 - 210 °F | |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 90.6 - 98.9 °C | 195 - 210 °F | |
Diamond Polymers ABS/PC 9801 Description: Injection Molding Grade, High Impact, High HeatInformation provided by Diamond Polymers, Inc. |