Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP4-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Drying Temperature | 118 - 124 °C | 245 - 255 °F | |
Polymer Resources PCSF-FRG20 Polycarbonate, 20% Glass Reinforced Structural Foam Grade Polycarbonate, 20% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |