Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 105 - 115 °C @Time 10800 - 14400 sec |
221 - 239 °F @Time 3.00 - 4.00 hour |
Pre-dry |
Kingfa PC-S809 Modified PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Drying Temperature | 105 - 115 °C | 221 - 239 °F | Injection Molding |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Drying Temperature | 105 °C | 221 °F | |
Lubrizol Estane® ZHF 82AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 82AT0 NAT021 is an 82A aromatic polyether-based, non-halogen flame retardant, thermoplastic polyurethane (TPU) compound.Features: Soft, matte finished, good flame retardant proper.. |
|||
Drying Temperature | 105 °C | 221 °F | dehumidifying hopper |
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy sys.. |
|||
Drying Temperature | 105 °C | 221 °F | dehumidifying hopper |
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU Description: Stat-Rite® S1100 is a static dissipative TPU alloy. Stat-Rite S-1100 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD p.. |
|||
Drying Temperature | 105 °C | 221 °F | dehumidifying hopper |
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD .. |
|||
Drying Temperature | 105 °C | 221 °F | |
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an in.. |
|||
Drying Temperature | 105 °C | 221 °F | |
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in.. |
|||
Drying Temperature | 105 °C | 221 °F | |
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |
|||
Drying Temperature | 105 °C | 221 °F | |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |